Pacote de carretel com caixa de papelão, pacote de bobina com polybag, pacote de caixa de madeira
Habilidade da fonte:
1200 toneladas por mês
Destacar:
High Purity Superalloy Plate
,
10-60mm Nimonic 80A Plate
,
Nuclear Power Fasteners Superalloy Plate
Descrição do produto
Explore our precision hot rolled Nimonic 80A heavy superalloy plates ranging from 10mm to 60mm in thickness. Tailored specifically for mission-critical nuclear power fasteners and extreme stress environments requiring exceptional creep resistance and dimensional integrity. Product Overview: High Purity Nimonic 80A Plate Metallurgy Nimonic 80A is a premium nickel-chromium matrix alloy strengthened by precisely controlled additions of titanium and aluminum to form uniform gamma